Abstract

Weathering steel manufactured with high concentrations of copper (0.5wt%), chromium (0.5wt%) and nickel (2.4wt%) was studied with the aim of furthering knowledge on corrosion product characterization and performance in marine environments. Specimens exposed for two years in a rural atmosphere and two marine environments were characterized by optical microscopy, SEM/EDS, XRD and Raman spectroscopy and corrosion rates measured. The main phases found were ferrihydrite, maghemite and goethite in the inner corrosion layer, and lepidocrocite in the outer layer. Cu and Ni were homogeneously distributed while Cr tended to be concentrated in the inner layer.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.