Abstract
Degradation of materials due to solid particle erosion is encountered in a variety of engineering industries, either at room temperature or elevated temperatures. Nickel-based coatings are commonly used in applications where wear resistance, combined with oxidation or hot corrosion resistance, is required. In the present work, NiCrAlY and Ni-20Cr metallic coatings were deposited on an iron-based superalloy by a shrouded plasma spray process. The coatings were characterized by scanning electron microscopy, optical microscopy, microhardness testing, and x-ray diffractometry. Erosion studies were conducted using an air-jet erosion test rig at a velocity of 40ms−1 and impingement angles of 30 and 90deg. Scanning electron microscopy was used to analyze the eroded surfaces. 3D surface roughness profiles of the eroded samples were taken using a Veeco Optical Profilometer. NiCrAlY coatings had slightly lower average porosity and lower microhardness as compared to Ni-20Cr coatings. The observed erosion rate of the NiCrAlY coatings, however was lower than that of the Ni-20Cr coatings at both 30 and 90deg impingement angles. Ni-20Cr coating had shown higher erosion rate at 90deg impingement angle than that at 30deg, whereas the effect of impingement angle on the erosion rate is negligible for plasma sprayed NiCrAlY coating. The higher bond strength of NiCrAlY coating might be one of the major contributing factors for lower erosion rate of NiCrAlY coating as compared to Ni-20Cr coating under the tested conditions. Erosion mechanisms of plasma sprayed coatings are discussed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.