Abstract

The performance of V2O5/TiO2-based commercial SCR catalyst for the oxidation of gaseous elemental mercury (Hg0) with respect to reaction conditions was examined to understand the mechanism of Hg0 oxidation on SCR catalyst. It was observed that a much larger amount of Hg0 adsorbed on the catalyst surface under oxidation condition than under SCR condition. The activity of commercial SCR catalyst for Hg0 oxidation was negligible in the absence of HCl, regardless of reaction conditions. The presence of HCl in the reactant gases greatly increased the activity of SCR catalyst for the oxidation of Hg0 to oxidized mercury (Hg2+) such as HgCl2 under oxidation condition. However, the effect of HCl on the oxidation of Hg0 was much less under SCR condition than oxidation condition. The activity for Hg0 oxidation increased with the decrease of NH3/NO ratio under SCR condition. This might be attributed to the strong adsorption of NH3 prohibiting the adsorption of HCl which was vital species promoting the oxidation of Hg0 on the catalyst surface under SCR condition.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.