Abstract

The present study describes the application of CZE to investigate the portion of labile iron in the following parenteral formulations: iron gluconate, iron saccharate, and iron dextran. Labile iron was detected as Fe(III)-chelate of EDTA at 246 nm. When EDTA was incubated with the formulations before electrophoresis, labile iron, or chelatable iron, respectively, was detected in all formulations, mostly in iron gluconate and iron saccharate. It was observed that the amount of iron released is time- and pH-dependent. In contrast, when EDTA was separately injected before the formulation sharp peaks of the Fe(III)-chelate were detected only after injection of iron gluconate. This type of labile iron can be described as "electrophoretically free" iron. CE provides thus a new method to characterize potential toxic, labile iron in parenteral iron formulations.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.