Abstract

Silicon nanowire samples fabricated by thermal evaporation of SiO powder were investigated by Cathodoluminescence. Three main bands were found at low temperatures, namely, peak 1 at about 620–650 nm (2.0–1.91 eV), peak 2 at 920 nm (1.35 eV), and peak 3 at 1280 nm (0.97 eV). An additional broad band (peak 4) in the infrared region with its maximum at ∼1570 nm (0.79 eV) appears at room temperature. The origins of the emission bands are discussed.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.