Abstract
To develop an efficient catalyst for steam reforming of propane, Ni/LaAlO3 catalysts were prepared by deposition precipitation, impregnation, and solvo-thermal methods, and characterized by XRD, BET, H2-TPR, elemental analyses, and TEM. Ni/Al2O3 and Ni/CeO2 catalysts were also synthesized by the solvo-thermal method for comparison. The Ni/LaAlO3 catalysts exhibited better catalytic performance than both Ni/Al2O3 and Ni/CeO2 catalysts, and activities with Ni/LaAlO3 were found to be dependent upon the preparation methods. In particular, the Ni/LaAlO3 catalyst synthesized by the solvo-thermal method exhibited the highest activity presumably because tetrahydrofuran helps distribute generated Ni nanoparticles onto the catalyst surface in a uniform fashion. In addition, the solvo-thermally prepared Ni/LaAlO3 catalyst was found to be highly stable, with its activity being maintained at least during 100 h. The observed high stability is attributed to the excellent oxygen storage capacity of LaAlO3, which was first determined by thermogravimetric methods as well as by soot oxidations in the presence of Al2O3, CeO2, and LaAlO3. Compared to the Ni/Al2O3 and Ni/CeO2 catalysts, Ni/LaAlO3 exhibited suppressed carbon formation even at lower S/C ratios due to the superior oxygen transport ability of the LaAlO3 support.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.