Abstract

Abstract The H sorption properties of mixtures Mg + WO 3 (having various structures) and Mg + H 0.23 WO 3 are reported. First, the higher conversion of Mg into MgH 2 during reactive mechanical grinding (under 1.1 MPa of H 2 ) for higher WO 3 content is due to the improvement of the milling efficiency. Then, it is shown that the hydrogen absorption properties are almost independent of the crystal structure of the catalyst and that only the particles' size and the specific surface play a major role. Finally, for the desorption process, it appears that the chemical composition and structure of the catalyst, together with the particle size and specific surface have an effect.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.