Abstract

In this study, the effect of graphite on sphalerite dissolution was investigated using a Leptospirillum ferrooxidans (L. ferrooxidans) dominated meso-acidophilic bacterial consortium. Results of the studies indicated that Zn dissolution enhanced from 18.75% (in control tests) to 78.46% (using L. ferrooxidans) without graphite in the system (the conventional approach). Addition of graphite further improved sphalerite bio-oxidation up to 10%, i.e., from 78.46 to 87.83% indicating bio-catalytic effect and possible galvanic interaction between sphalerite and graphite. Through the conventional route, the system’s pH eventually lowered from 1.8 to 1.4 and ORP increased from 300 to 700 mV. In presence of graphite, the pH lowered to nearly 1.0 and ORP reached 600 mV. This indicated efficient bacterial activity and stabilized leaching conditions in both cases. Analytical characterization studies through XRD and SEM-EDAX indicated the presence of sulfur and K-type jarosite (KFe3+ 3(OH)6(SO4)2), ascribed to the passivation layers formed during sphalerite bioleaching.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.