Abstract

Catalytic depolymerization of organosolv lignin to phenolic monomers with zeolites was investigated under various operating conditions. H-USY (Si/Al molar ratio = 5) outperformed H-USY with Si/Al ratios of 50 and 250, H-BEA, H-ZSM5, and fumed SiO2 to produce the highest phenolic monomer yield from a commercial organosolv lignin in methanol at 300 °C for 1 h. It was then further investigated in the presence of acetone, ethyl acetate, methanol, and methyl isobutyl ketone (MIBK) on the depolymerization of organosolv bagasse lignin (BGL). The total highest phenolic monomer yield of 10.6 wt % was achieved with MIBK at 350 °C for 1 h with a catalyst loading of 10 wt %. A final total phenolic monomer yield of 19.4 wt % was obtained with an initial H2 pressure of 2 MPa under similar processing conditions. The main phenolic monomers obtained are guaiacol (7.9 wt %), 4-ethylphenol (6.0 wt %), and phenol (3.4 wt %). The solvent properties were used to account for the differences in phenolic monomer yields obtained w...

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.