Abstract

TiO2 and La-doped TiO2 samples with La loading between 0.2% and 2% have been prepared, characterised, and tested in the catalytic oxidation of soot by O2. La doping prevents anatase to rutile phase transformation and crystallite size growth when heated at 800°C, as deduced from XRD, Raman spectroscopy and BET surface area measurements. The optimum La loading was found to be 0.2%. The catalytic activity of TiO2 and La-doped TiO2 samples tested mainly depends on crystallite size, the lower the size the better the activity. TiO2 phase composition is not a key factor in the catalytic oxidation of soot.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.