HighlightsNi3Fe oxide, with an average size of 3.5 ± 1.5 nm, was successfully deposited onto polyaniline (PANI) support through a solvothermal strategy followed by calcination.The catalyst–support interaction between Ni3Fe oxide and PANI can enhance the Ni-O covalency via the interfacial Ni-N bond.Ni3Fe oxide/PANI-assembled Zn-air batteries achieve superior cycling life for over 400 h at 10 mA cm−2 and a low charge potential of around 1.95 V.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.