Abstract
Grain size and microstructural features of cast superalloy K4169 were investigated under various melting and casting conditions together with the addition of grain refiners. It is found that lowering the pouring temperature and adding refiners to the melt before pouring can lead to grain refinement of �� matrix and improve the proportion of equiaxed grains. At a conventional pouring temperature of 1400 �� , the average size of equiaxed grains could be refined to the order of ASTM 3.2 (0.17 mm), the proportion of equiaxed grains at the transverse cross-section could be improved from 56% to 99% with addition of a trace intermetallic compound into the melt. The results also indicate that the length of primary dendrite is shortened with the addition of refiners, but the secondary dendrite arm spacing keeps almost unchanged. Meanwhile, the microsegregation of main elements such as Fe, Cr, Nb, Mo and Ti is alleviated with the decrease in grain size, and the grains have transformed from dendrite to granulation in fine-grained castings. The amount of microporosity in samples with the addition of refiners can be greatly reduced. The mechanisms of grain refinement and increase in equiaxed grain proportion were proposed.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.