Abstract

Mesh size distributions (MSDs) of swollen cross-linked styrene copolymer networks have been measured by thermoporometry using CCl(4) as a probe liquid. All numerical relationships required for the calculation of the MSD were established for both the liquid-to-solid and the solid-to-solid thermal transitions of CCl(4) and successfully validated on test samples. It was found that the polymer network, for both thermally and photo-cross-linked materials, was completely built in about 4 h of exposure. A clear correlation was established between the average mesh size of the swollen polymer network on one hand and the benzoyl peroxide groups content and swelling ratio on the other hand.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.