Abstract

AbstractNd‐doped PbClF crystals were grown with modified Bridgman method. Broad and flat emission band at 1.0 μm was observed. The FWHM value of 0.0091 wt.% Nd3+‐doped PbClF crystal at 1064 nm reached up to 30 nm with the peak emission cross‐section of 1.05×10‐19 cm2. All the results indicated that Nd‐doped PbClF crystal should be a promising tunable and ultrafast laser material. (© 2012 WILEY‐VCH Verlag GmbH & Co. KGaA, Weinheim)

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.