Neutral sulphite pulping of softwood as a potential biorefinery was investigated, by producing pulps at two main yield levels (55–65% and 75–85%) under various process conditions and by analysing the composition of the resulting fibre fractions and pulping spent liquors. It was found that both delignification rate and selectivity were enhanced by addition of anthraquinone (AQ 0.1% on o.d. wood) whereas delignification was accelerated by higher temperature (180 °C vs. 170 °C) and initial liquor pH (10 vs. 7). The established conditions preserved significant amount of carbohydrates, especially galactoglucomannan, in the fibres at the selected yield levels. At the yield level of 65%, still over 60% of galactoglucomannan was detected in the pulps whereas 50–70% of lignin was removed. In the spent liquors, lignosulphonates as the principal component represented the possible source of by-product in addition to acetic and formic acids.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.