Abstract
In this paper, the cavitation erosion respectively the dry sliding wear behaviour of the Ysn83 antifriction alloy and EN-GJS-400-15 spheroidal cast iron was studied. As cavitation erosion aspects, the authors show some preview results of the Ysn83 antifriction alloy behaviour and continue to study and to compare also the cavitation erosion behaviour of the EN-GJS-400-15 spheroidal cast iron. In this regard, the cavitation erosion tests were made using a cavitation stand and the experimental results were presented through mass loss and cavitation erosion rate vs time curves. As dry sliding wear aspects, the tests for the two investigated materials were done with a tribometer through the pin-on-disk method where the authors varied the parameters especially the linear speed and the distance. The obtained results were presented as coefficient of friction evolutions and as wear rates. From all the tests, compared with the YSn83 antifriction alloy, the EN-GJS-400-15 spheroidal cast iron showed a superior cavitation erosion and dry sliding wear behaviour.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: IOP Conference Series: Materials Science and Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.