Abstract

Thermoplastic poly(ester-siloxane)s (TPES) and poly(ester-ether-siloxane) s, (TPEES), based on poly(butylene terephthalate) (PBT) as the hard segment and different siloxane-prepolymers as the soft segments, were prepared. The TPES and TPEES were synthesized by catalyzed two-step transesterification from dimethyl terephthalate, (DMT), 1,4-butanediol, (BD) and a siloxane-prepolymer. Incorporation of dicarboxypropyl- or disilanol-terminated poly(dimethylsiloxane)s (PDMS) into the polar poly(butylene terephthalate) chains resulted in rather inhomogeneous TPES copolymers, which was a consequence of a prononuced phase separation of the polar and non-polar reactants during synthesis. Two concepts were employed to avoid or reduce phase separation: 1) the use of siloxane-containing triblock prepolymers with hydrophilic terminal blocks, such as ethylene oxide (EO), poly(propylene oxide) (PPO) or poly(caprolactone) (PLC) when the terminal blocks serve as a compatibilizer between the extremely non-polar PDMS and the polar DMT and BD, and 2) the use of a high-boiling solvent (1,2,4-trichlorobenzene) during the first phase of the reaction. Homogeneity was significantly improved in the case of copolymers based on PCL-PDMS-PCL. .

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.