1. Intermediate annealing after stamping large preforms of steel 30KhGSNMA-VD can be accompanied by temper brittleness of kind II, which causes the formation of brittle cracks in subsequent grinding and quenching. 2. In order to prevent the formation of brittle cracks in stamped preforms, they should be subjected to sandblasting after grinding and decelerated heating for quenching in the final treatment.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.