Abstract

The aim of the study was to analyze the properties of foamed bitumen produced from 50/70 bitumen in terms of the assessment of its usefulness to the road construction materials. In order to improve the foaming parameters the synthetic wax Fischer-Tropsch (FT) in an amount of 1.0%, 2.0% and 3.0% was used. Bitumen binder parameters were evaluated before and after the foaming process. The basic parameters were evaluated (before the foaming process): penetration, Fraass breaking point and softening point. The bitumen foam parameters were measured at the foaming water content (FWC) in the range from 1.5% to 4.0% with an increment of 0.5%. The tests allowed determining optimal application ranges for the FT and the FWC to produce asphalt at lower temperatures.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.