PPTA fibers made by China ShenMa Group Co., Ltd and Kevlar49 fibers made by Dupont as experimental materials were used in this paper. The differences of molecule structures were contrasted through infrared spectrum and degree of polymerization-counting by the detections of viscosity. The PPTA fibers were put into distilled water and seawater made by ourselves respectively, then ultrasonication were used to deal with them. After this, using the SEM to observe, found that the cracks appear on the fibers surfaces, presented the fibrillation and plush-like microfine fibers. Meanwhile the strength weak-link increased and breaking strength and elongation at break of fibers lowered after ultrasonication. Molecular kinetic theory was used in this paper to study loss of fibers the mechanical property.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.