Abstract

Pyroelectric materials can be used for energy harvesting in integrated Micro-Electro-Mechanical-Systems (MEMS) and low power electronics devices. This paper considers the thermal energy harvesting using Ca0.15(Sr0.5Ba0.5)0.85Nb2O5 (CSBN) pyroelectric ceramics. Hot/cold air was used to generate a continuous temporal temperature profile on the material surfaces. The maximum open circuit voltage was observed as 0.26V. The maximum stored energy was 1.9 μJ in 47 μF capacitor (without load resistance). The maximum power was found to be 2.07nW across 3 MΩ and 47 μF.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.