Abstract

The aim of this paper is to quantify mechanical fracture and length change parameters of the two types of concrete with alkali activated binder. The six beam specimens (75 × 75 × 295 mm) were made from each mixture. After demolding specimens were placed in air storage for 28 days. During this period length change (shrinkage) were recorded in accordance with ASTM C490 (2011). After that the three-point bending test was performed on these specimens with initial stress concentrator at the age of 28 days to obtain the mechanical fracture parameters. Records of fracture tests in form load versus deflection (F–d) diagrams were evaluated using effective crack model and work of fracture method.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.