Mechanical mixtures of zirconia gel and crystalline Y 2O 3 (3 mol%) have been hydrothermally treated at 110°C for 7 days in the presence of different mineralizer solutions. Taking the K 2CO 3/KOH molar ratio constant and equal 3, the total concentration of the mineralizer solutions was changed between 0.25 and 3.0 M. Predominant tetragonal (T) ZrO 2, characterized by different crystal size and different degree of agglomeration resulted by changing the concentration of mineralizer solution. The crystallization rate of Y-TPZ based powders, as well as the texture of the corresponding sintered products, are discussed in terms of concentration of the mineralizer solutions.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.