Abstract
SiO 2 and SnO 2 films were deposited using plasma-enhanced atomic layer deposition (PEALD) at low temperature (100 °C), and homogeneously mixed structure (HMS) films consisting of Si, Sn, and O were deposited through a “1st precursor dose – 2nd precursor dose – oxidation”, a new ALD process method for mixing two elements. For a deep consideration of the growth mechanism during the HMS film deposition process, density functional theory (DFT) calculations of the adsorption reactions of the precursors on the surface were conducted. The properties of the thin films such as density, atomic composition, crystallinity, surface roughness, optical transmittance and the water vapor diffusion barrier property were analyzed by XRR, XPS, XRD, AFM, UV-VIS and the electrical Ca test. By changing the dose sequence of the two precursors in the HMS process, various physical/chemical characteristics of the films could be controlled. Also, by adjusting the appropriate amount of Sn in the HMS films, the shortcomings of SnO 2 were compensated by the mixed SiO 2 ; and through this process, excellent gas diffusion barrier properties of WVTR ∼ 1.33 × 10 −4 g/m 2 day were secured.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.