Abstract

Mn and Si were magnetron co-sputtered on Si (100) substrates and annealed in the temperature range of 773-848 K in Ar atmosphere to obtain MnSi. The results were tested by XRD, high resolution SEM (HRSEM), 4 points probe measurements and AES. The activation energy calculated on the basis of XRD intensity is in the range of 0.43-0.71 eV. The Mehl-Johnson relation was applied for the determination of the activation energy interval. The HRSEM thicknesses evaluated are related to the intensity measurements. The constants appearing in the Mehl-Johnson equation were determined by graphical iteration. The activation energy calculated on the basis of film thickness is almost exactly the same as that obtained by XRD intensity measurements being in the range of 0.43 – 0.73. The results of the activation energy evaluation of MnSi formation and the method relating XRD intensities to the thickness are discussed.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.