Abstract

The direct conversion of celestite, SrSO 4, to strontium carbonate, SrCO 3, in leaching solutions of sodium carbonate, Na 2CO 3, wasanalyzed using an air-lift loop vessel or Pachuca tank (0.28 m I.D. × 1.36 m total height, 90° conical bottom) as reactor. The kinetics of the process were studied at 353 K (80 °C) using 1.1 M Na 2CO 3 solutions containing 18 wt % celestite particles. Experimental runs were carried out to determine the effects of particle size distribution (−106 and −250 μm) and geometrical and operating parameters of the reactor, such as draft tube diameter-to-reactor diameter ratio, D d/D t (0.25 and 0.5) and superficial air velocity, V sg (0.15 to 0.77 cm/s), respectively. The results showed that leaching rate was improved by increasing air superficial velocity and D d/D t ratio, and by decreasing particle size. For the same size distribution and air velocity, the kinetics were improved by increasing the D d/D t ratio. A shrinking-core model considering diffusion of CO 3 2− ions, through the solution contained in the pores of the strontium carbonate product layer, as the rate limiting stage gave a good description of the kinetics of the leaching process. Furthermore, the model takes into account both the particle size distribution of the treated samples and the depletion of leaching reactant that occurs as reaction proceeds.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.