<h2>Abstract</h2> The use of metal-on-metal low-wearing bearings has promoted great interest in the factors determining the volume of wear debris generated in such joints, including the developing surface replacement alternatives. Twenty-six pairs of low- and high-carbon components in wrought or cast form of 36 mm nominal diameter and exhibiting similar clearances were studied over 5 million test cycles in a 10-station hip joint simulator. Low-carbon cast materials exhibited higher wear than high-carbon cast or wrought materials. Little difference was found in the running-in wear volumes generated by high-carbon wrought or cast materials, but the wrought material exhibited a slight advantage at the smallest diametral clearance considered of 105 μm. Volumetric wear appeared to decrease as the diametral clearance decreased.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.