Abstract
Differential scanning calorimeter thermograms have been obtained for the alkali metal stearates from 25 to 200 °C. Four different samples of different thermal history were studied for each soap, and differences in temperature and relative enthalpy of transitions were found to depend on the various sample histories. For lithium stearate good correlation is found between DSC and nuclear magnetic resonance (n.m.r.) results. Rubidium and caesium stearates seem to be less sensitive to thermal history than the sodium and potassium salts.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.