Abstract

Abstract The paper presents the results of a theoretical investigation whose objective has been to see whether there are advantages to be gained from using the modified J-integral in procedures for estimating the critical crack length for CANDU pressure tubes. For typical operation conditions, and with irradiated tubes having critical crack lengths over a wide range, it is shown that the slope of the modified J-integral JM-Δa crack growth resistance curve for a pressure tube crack is only marginally greater than the slope of the corresponding deformation J-integral JD-Δa curve; the results are expressed in terms of the parameter Z ∗ , which is dJM/da − dJD/da and the parameter Q, which is the fractional difference between dJM/da and dJD/da. In the light of these findings, there would appear to be little advantage to be gained in using JM, rather than JD, as a characterizing parameter for crack growth in a CANDU pressure tube.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.