Objective: The aim of this study was to determine, in vitro, the relative short- and long-term fluoride release from four resin-modified glass ionomers (Fuji II LC, Vitremer, Enforce & Advance), a polyacid-modified composite resin (Dyract compomer) and a bonding agent (OptiBond). Methods: All the materials were prepared as outlined by the manufacturers. Circular discs of the materials mentioned were suspended in water for up to 300 days and the non-cumulative 24-h fluoride release was determined potentiometrically at chosen times. Results: The amounts of fluoride released during the first day were Vitremer (1.46 μg mm −2), Advance (1.18 μg mm −2), Fuji (1.08 μg mm −2), Optibond (0.33 μg mm −2), Dyract (0.31 μg mm −2) and Enforce (0.15 μg mm −2). After the second day the sequence changed slightly and remained approximately the same for the rest of the 300-day period. There was also an increase in the fluoride release during the 60–200-day period relative to the previous period. Conclusion: In general the most fluoride was released by Advance and not by Fuji II LC or Vitremer. For most materials, fluoride is still released after 300 days. Furthermore, even a thin layer of bonding agent released a relatively high amount of fluoride (volume-wise the most) at the beginning. It is deduced that even the release of relatively low amounts of fluoride may result in significant concentrations of fluoride in a microleakage gap.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.