Abstract

This paper presents micro-OBIC measurements performed at different voltages on two devices protected by narrow field rings. At the surface of the device #1, a polyimide layer was deposited during the fabrication process. On the contrary, passivation layer was removed on device #2. Thanks to the micro-OBIC micrometer spatial resolution and the spot size carefully focused, small gaps in the range of 1 μm can be visible on OBIC profiles. Thus, the variation of the μ-obic accurately reflects the topology of each ring.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.