Abstract
For specimen characterization, X-ray microscopy offers a variety of advantages like non-destructive investigations and reduced preparation effort for the samples. Orientation measurements are possible using diffraction contrast tomography (DCT). However, lateral resolution is lower as compared to scanning electron microscopy combined with electron backscatter diffraction (EBSD). A sample of a nickel-based superalloy IN738LC was investigated three-dimensionally for direct comparison of EBSD and DCT, which clearly reveals the advantages, disadvantages and limits of both methods. Images obtained by EBSD showed more microstructural details, but also artefacts resulting from the previous sample preparation. DCT seemed more suitable for 3D-imaging, but was not able to resolve some of the smaller grains.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.