Abstract

AbstractA facile method to identify the moisture content in overcoat (OC) of CF is demonstrated herein. The authors provide efficient methods to lower the water percentage in OC and the possible mechanism is proposed. LCD manufacturers could thus efficiently reduce the risk of bubbles and raise yields.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.