Abstract

. The physicochemical changes of refined vernonia oil?RVO (which naturally contains epoxidized triglycerides) upon heating was evaluated and is reported in this manuscript. A boiling point range of 183 °C to 190 °C (at 760 mm Hg) for the vernonia oil was obtained using the Siwolobboff's method. The oil changed its physical appearance and consistency in the course of the heating. A homogenous free?flowing beige?sand shade refined vernonia oil at room temperature (25 °C) was transformed irreversibly to an intense?brown shade, becoming increasingly more viscous with increase in temperature, and ceasing to flow momentarily at 188 °C. On cooling to room temperature, the oil solidified into a brown rubber?like elastic material. The oil also exhibited a reduction in its oxirane content from 1.39±0.004 equivalent HBr kg?l at 25 °C to 0.542±0.002 equivalent HBr kg?l at 70 °C. This signifies a 61% drop in oxirane content for the 45 °C temperature rise. These findings point towards a thermally driven polymerization and/or decomposition of the refined vernonia oil (RVO). (Received May 20, 2000, revised December 13, 2000) Bull. Chem. Soc. Ethiop. 2000, 14(2), 161-168

Highlights

Read more

Summary

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.