Abstract

(1-x)(K0.44Na0.52Li0.04)(Nb0.84Ta0.10Sb0.06)O3-xSrTiO3 (KNNT-ST) lead free piezoelectric ceramics have been synthesized by a solid state reaction method. The effect of SrTiO3 content on the piezoelectric properties, sintering behavior and microstructure of (1-x) KNNT-x ST ceramics was investigated. The experimental results showed that the addition of SrTiO3 can restrain the volatilization of Na ions and K ions and improve relative density of the samples. A morphotropic phase boundary between orthorhombic and tetragonal phases is found in the composition range of 0.03<x<0.05. The piezoelectric properties can be enhanced for (1-x) KNNT-x ST ceramics near the morphotropic phase boundary.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.