Abstract
05/00037 Development of a new oxidation stability test method for lubricating oils using high-pressure differential scanning calorimetry: Sharma, B. K. and Stipanovic, A. J. Thermochimica Acta, 2003, 402, (12), 1–18
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.