Abstract
The residual stress and various characteristics of Ti-N films coated on the surface of SKH51 substrate by ion beam mixing technique were examined. As a result, it was found that the wear characteristic of the films in which Ti2N phase coexisted with TiN phase was better than that of the TiN single phase films, though the dynamic hardness of the former films was lower than that of the latter films. When a small amount of Ti2N phase existed in TiN phase matrix, both the residual stress and the particle size of TiN phase showed a minimum. As to the TiN+Ti2N two phase films coated with the same N/Ti supply ratio, the specific wear rate was decreased when the residual stress of the film was increased.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of the Society of Materials Science, Japan
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.