Abstract
In using CR-39 plastics for individual neutron dosimeters, changes of etching efficiency cause significant error in dose estimation. Etching efficiency is subject to a number of parameters. In this study the influences of the parameters were examined by measuring the diameters of etch-pits formed by alpha-particles and enlarged by aqueous solutions of 25-35% KOH at 55-65°C for 4hr. It has been observed that diameter changes at the rate of 8.3%/°C in temperature, 8.2%/wt% in concentration and -0.60%/day in time after preparation of etchant. The diameter is unaffected by the supplying of up to 280ml/l, of distilled water for evaporation of etchant or by increase up to 5g/l of CR-39 dissolved in etchant. The magnitude of possible error has been estimated by parameter as well as ingeneral, so as to obtain suggestions for improving etching treatment.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.