Magnetic properties of iron nitride thin films as well as Fe4N/Fe multilayered films prepared by a reactive plasma deposition method have been investigated. The Fe4N single phase was produced under PN2=4mTorr, substrate temperature=above 300°C and output power of r.f. generator=above 300W.The multilayered films consisting of Fe/Fe4N/Fe as well as Fe4N/Fe/Fe4N were deposited by control-ling the plasma power. The saturation magnetization of the multilayered films mainly depended on the thickness of the Fe layers. The coercive force of the films was greater than that of the Fe single phase because of nitrogen from the Fe4N layer was diffused into the Fe layer. The film, of a small coercive force of 29 Oe, containing little nitrogen in the Fe layer was made when the deposition rate of the iron in the Fe4N/Fe/Fe4N multilayered film became speeded up.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Journal of the Japan Society of Powder and Powder Metallurgy
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.