Composite coatings consisting of SiC particles of 1, 5 and 10μm, codeposited into an electroless nickel matrix were produced, and their physical properties were sutdied. The hardness of the coatings increased with increasing SiC content, and remained about equal for coatings of the same SiC content irrespective of particle size. The coatings were found to have excellent wear resistance, but this decreased with increased in particle size, and with heat treatment at 673K. The coatings were also found to have excellent wear resistance when applied to parts of a wire twisting machine.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.