Abstract

Mechanical properties of work hardened pure titanium joint brazed with Ti-Cu-Cr-Al filler metal were investigated.Test specimens were brazed with filler metal containing 29%Ti, 62.5%Cu, 6.5%Cr and 2%Al in a vacuum. Brazing temperature were 850°C, 900°C, 1, 000°C and 1, 100°C for 10sec. Tensile strength of butt joints were comparable to that of joints brazed with conventional Ti-Ni-Cu filler metal, and hardness at the joint was lower. The reaction of filler metal with base metal was modertely and damage of base metals were less. The addition of pressure to joint during brazing gave significant effect on joint strength.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.