Abstract

High-coercivity anisotropic magnet powder of HcJ=1.24MA/m has been developed in HDDR process by substituting Dy for Nd to decrease the value of irreversible thermal flux losses. The newly developed powder provides lower irreversible thermal losses than MQP-B up to 100°C when molded into resin-bonded magnets. The magnets made from the high-HcJ powder give higher relative open flux when magnetized under a magnetization field of 1.2MA/m at 80°C than magnetized at 20°C. To magnetize these magnets at high temperature also decreases the value of irreversible thermal flux losses.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.