The decrease of the rolls wear is an important reserve of the improvement of rolling production. At present during rolling metal of all kinds at the wide-strip rolling mill CWRM-1700 by the JSC “ArselorMittal Temirtau” work rolls of the Hi-Cr type are used in stands No. 6–8, whereas work rolls of the ICDP type are used in stands No. 9–12 for finish rolling. Initial and worn profiles of rolls were determined using the instrument ID 05009. Measurements were performed after roll reloading and cooling, mainly before polishing, with the accuracy of ± 0.01 mm. The amount, assortment and steel grades of the rolled metal, as well as diameters, chemical composition and hardness of the rolls were also fixed. In general research permitted to estimate the wear of the work rolls of the finishing group of CWRM-1700 using geometrical, kinematic and energy indicators of wear. The energy indicator is universal since it takes into account the decrease of the body size from unit work of friction forces on unit roll surface. The kinematic indicator takes into account the decrease of the roll radius relative to unit friction path of the roll surface. The change of geometrical wear indicators of rolls with the same properties in different stands makes it necessary to take account of technological factors that were taken into account while calculating kinematic and energy indicators.
Highlights
Уменьшение изнашиваемости валков – важный резерв совершенствования прокатного производства
In general research permitted to estimate the wear of the work rolls of the finishing group of CWRM-1700 using geometrical, kinematic and energy indicators of wear
The energy indicator is universal since it takes into account the decrease of the body size from unit work of friction forces on unit roll surface
Summary
Уменьшение изнашиваемости валков – важный резерв совершенствования прокатного производства. В настоящее время при прокатке на стане НШПС-1700 АО «АрселорМиттал Темиртау» металла всех назначений в клетях чистовой группы No 6–8 используются рабочие валки исполнения Hi-Cr, а в клетях No 9–12 – валки исполнения ICDP. В целом в работе проведена оценка изнашиваемости рабочих валков чистовой группы НШПС-1700 с использованием геометрического, кинематического и энергетического показателей изнашиваемости. Энергетический показатель изнашиваемости универсален, так как учитывает уменьшение размера тела от единицы работы сил трения на единице поверхности валка.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: Bulletin of the South Ural State University Series ‘Metallurgy’
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.